Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.74 g/cm³ Show Supplier Material materials with Dichte of 1.74 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | 50%RH | ISO 62 | 2 mm | |
Sauerstoffindex | 23 °C | 45 % Show Supplier Material materials with Sauerstoffindex of 45 % | ISO 4589-2 | |||
Wasserabsorption | 2.5 % Show Supplier Material materials with Wasserabsorption of 2.5 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 130 MPa Show Supplier Material materials with Biegefestigkeit of 130 MPa | 50%RH | ISO 178 | 2mm/min | |
240 MPa Show Supplier Material materials with Biegefestigkeit of 240 MPa | dry | ISO 178 | 2mm/min | ||
Biegemodul | 7.9 GPa Show Supplier Material materials with Biegemodul of 7.9 GPa | 50%RH | ISO 178 | 2mm/min | |
14 GPa Show Supplier Material materials with Biegemodul of 14 GPa | dry | ISO 178 | 2mm/min | ||
Dehnung | 2.1 % Show Supplier Material materials with Dehnung of 2.1 % | dry | ISO 527-2/1A | 5mm/min | |
2.3 % Show Supplier Material materials with Dehnung of 2.3 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 8.8 GPa Show Supplier Material materials with Elastizitätsmodul of 8.8 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
14.6 GPa Show Supplier Material materials with Elastizitätsmodul of 14.6 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | 50%RH | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | dry | ISO 179/1eU | |
23 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | 50%RH | ISO 179/1eU | ||
Zugfestigkeit | 95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
155 MPa Show Supplier Material materials with Zugfestigkeit of 155 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | 1 mm, 2 mm | IEC 60695-2-12 | ||||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | ISO 11357-1/-3 | 10°C/min | ||||
Entflammbarkeit | Thickness tested (mm): 1.6, Class: V-0, Standard: UL 94 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | 310/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.8 % Show Supplier Material materials with Schrumpfung of 0.8 % | 310/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent, Flame retarding agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Natural | |
Features | Flame Retardant, Halogen-free, Phosphorus-free, Heat Stabilized | |
Fillers | 25% Glass Fiber | |