Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.55 g/cm³ Show Supplier Material materials with Dichte of 1.55 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1 % Show Supplier Material materials with Moisture absorption of 1 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 4 % Show Supplier Material materials with Wasserabsorption of 4 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 190 MPa Show Supplier Material materials with Biegefestigkeit of 190 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 9.3 GPa Show Supplier Material materials with Biegemodul of 9.3 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 2.1 % Show Supplier Material materials with Dehnung of 2.1 % | dry | ISO 527-2/1A | 5mm/min | |
2.5 % Show Supplier Material materials with Dehnung of 2.5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 9.1 GPa Show Supplier Material materials with Elastizitätsmodul of 9.1 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
9.8 GPa Show Supplier Material materials with Elastizitätsmodul of 9.8 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | 50%RH | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | dry | ISO 179/1eU | |
23 °C | 43 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 43 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 45 kJ/m² | 50%RH | ISO 179/1eU | ||
Zugfestigkeit | 90 MPa Show Supplier Material materials with Zugfestigkeit of 90 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Testing Standard | Thickness | Comment | |||
---|---|---|---|---|---|---|---|
Ball pressure temperature | 185 °C Show Supplier Material materials with Ball pressure temperature of 185 °C | IEC 60695-10-2 | |||||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | IEC 60695-2-12 | 1 mm, 2 mm | ||||
Glow Wire Ignition Temperature | 850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | IEC 60695-2-13 | 1 mm, 2 mm | ||||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat-Erweichungstemperatur | 240 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 240 °C | ISO 306 | 50°C/h 50N | ||||
Wärmeformbeständigkeitstemperatur | 225 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 225 °C | ISO 75/2Af | 1.80 MPa | ||||
Entflammbarkeit | Thickness tested (mm): 0.8, Class: V-0, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1 % Show Supplier Material materials with Schrumpfung of 1 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent, Flame retarding agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Natural | |
Features | Flame Retardant, Heat Stabilized | |
Fillers | 25% Glass Fiber | |
Processing methods | Injection Molding |