Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.14 g/cm³ Show Supplier Material materials with Dichte of 1.14 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 8.4 % Show Supplier Material materials with Wasserabsorption of 8.4 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 110 MPa Show Supplier Material materials with Biegefestigkeit of 110 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 2.9 GPa Show Supplier Material materials with Biegemodul of 2.9 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 40 % Show Supplier Material materials with Dehnung of 40 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
50 % Show Supplier Material materials with Dehnung of 50 % | 50%RH | ISO 527-2/1A | 50mm/min | nominal | ||
Elastizitätsmodul | 1.6 GPa Show Supplier Material materials with Elastizitätsmodul of 1.6 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
3.2 GPa Show Supplier Material materials with Elastizitätsmodul of 3.2 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation at yield | 4.5 % Show Supplier Material materials with Elongation at yield of 4.5 % | dry | ISO 527-2/1A | 50mm/min | |
25 % Show Supplier Material materials with Elongation at yield of 25 % | 50%RH | ISO 527-2/1A | 50mm/min | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | 50%RH | ISO 179/1eA | ||
Streckgrenze | 60 MPa Show Supplier Material materials with Streckgrenze of 60 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
85 MPa Show Supplier Material materials with Streckgrenze of 85 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 750 °C Show Supplier Material materials with Glow Wire Flammability Index of 750 °C | 2 mm | IEC 60695-2-12 | ||||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat-Erweichungstemperatur | 240 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 240 °C | ISO 306 | 50°C/h 50N | ||||
Wärmeformbeständigkeitstemperatur | 75 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 75 °C | ISO 75/2Af | 1.80 MPa | ||||
195 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 195 °C | ISO 75/2Bf | 0.45 MPa | |||||
Entflammbarkeit | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | 290/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.3 % Show Supplier Material materials with Schrumpfung of 1.3 % | 290/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse | |
Viscosity number | 260 cm³/gr Show Supplier Material materials with Viscosity number of 260 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Natural | |
Features | Heat Stabilized | |
Processing methods | Injection Molding,Profile Extrusion |