Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.22 g/cm³ Show Supplier Material materials with Dichte of 1.22 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 6 % Show Supplier Material materials with Wasserabsorption of 6 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 310 MPa Show Supplier Material materials with Biegefestigkeit of 310 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 13.5 GPa Show Supplier Material materials with Biegemodul of 13.5 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | dry | ISO 527-2/1A | 5mm/min | |
3.5 % Show Supplier Material materials with Dehnung of 3.5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 10.2 GPa Show Supplier Material materials with Elastizitätsmodul of 10.2 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
16.5 GPa Show Supplier Material materials with Elastizitätsmodul of 16.5 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | dry | ISO 179/1eU | |
23 °C | 75 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 75 kJ/m² | 50%RH | ISO 179/1eU | ||
Zugfestigkeit | 150 MPa Show Supplier Material materials with Zugfestigkeit of 150 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
215 MPa Show Supplier Material materials with Zugfestigkeit of 215 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | 1000 mm | ISO 11357-1/-3 | 10°C/min | |||
Entflammbarkeit | Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): <10 ,method: ISO 3795 and thickness tested (mm): 3 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Volume resistivity | 100 Ω·cm Show Supplier Material materials with Volume resistivity of 100 Ω·cm | dry, 50%RH | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Increased Electrical Conductivity | |
Fillers | 20% Carbon Fiber | |
Processing methods | Injection Molding |