Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.45 g/cm³ Show Supplier Material materials with Dichte of 1.45 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 5.7 % Show Supplier Material materials with Wasserabsorption of 5.7 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 150 MPa Show Supplier Material materials with Biegefestigkeit of 150 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 6.2 GPa Show Supplier Material materials with Biegemodul of 6.2 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 8 % Show Supplier Material materials with Dehnung of 8 % | dry | ISO 527-2/1A | 5mm/min | |
15 % Show Supplier Material materials with Dehnung of 15 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 3.1 GPa Show Supplier Material materials with Elastizitätsmodul of 3.1 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
6 GPa Show Supplier Material materials with Elastizitätsmodul of 6 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5.5 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | 50%RH | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 55 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 55 kJ/m² | dry | ISO 179/1eU | |
23 °C | 70 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 70 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | 50%RH | ISO 179/1eU | ||
Zugfestigkeit | 45 MPa Show Supplier Material materials with Zugfestigkeit of 45 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
87 MPa Show Supplier Material materials with Zugfestigkeit of 87 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | 2 mm | IEC 60695-2-12 | ||||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat-Erweichungstemperatur | 245 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 245 °C | ISO 306 | 50°C/h 50N | ||||
Wärmeformbeständigkeitstemperatur | 100 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 100 °C | ISO 75/2Af | 1.80 MPa | ||||
Entflammbarkeit | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Kriechstromfestigkeit | 500 V Show Supplier Material materials with Kriechstromfestigkeit of 500 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 1 % Show Supplier Material materials with Schrumpfung of 1 % | 290/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | 290/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Yellow Card, RoHS 2011/65/UE | |
Color | Black | |
Fillers | 40% Mineral Powder | |
Processing methods | Injection Molding |