Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness |
---|---|---|---|---|---|
Dichte | 1.09 g/cm³ Show Supplier Material materials with Dichte of 1.09 g/cm³ | dry | ISO 1183 | ||
Moisture absorption | 23 °C | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | 50%RH | ISO 62 | 2 mm |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 32 MPa Show Supplier Material materials with Biegefestigkeit of 32 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 0.94 GPa Show Supplier Material materials with Biegemodul of 0.94 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 100 % Show Supplier Material materials with Dehnung of 100 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
Elastizitätsmodul | 0.9 GPa Show Supplier Material materials with Elastizitätsmodul of 0.9 GPa | dry | ISO 527-2/1A | 1mm/min | |
Modulus at 50% elongation | 0.037 GPa Show Supplier Material materials with Modulus at 50% elongation of 0.037 GPa | dry | ISO 527-2/1A | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 97 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 97 kJ/m² | dry | ISO 179/1eA | |
Streckgrenze | 38 MPa Show Supplier Material materials with Streckgrenze of 38 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermisch
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Schmelzpunkt | 258 °C Show Supplier Material materials with Schmelzpunkt of 258 °C | ISO 11357-1/-3 | 10°C/min | ||
Entflammbarkeit | Thickness tested (mm): 3.2, Class: HB, Standard: UL 94 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Release agent, Plasticizer | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Impact Modified, Heat Stabilized | |
Processing methods | Injection Molding |