Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 7.8 % Show Supplier Material materials with Wasserabsorption of 7.8 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 125 MPa Show Supplier Material materials with Biegefestigkeit of 125 MPa | 50%RH | ISO 178 | 2mm/min | |
215 MPa Show Supplier Material materials with Biegefestigkeit of 215 MPa | dry | ISO 178 | 2mm/min | ||
Biegemodul | 3.5 GPa Show Supplier Material materials with Biegemodul of 3.5 GPa | 50%RH | ISO 178 | 2mm/min | |
5.8 GPa Show Supplier Material materials with Biegemodul of 5.8 GPa | dry | ISO 178 | 2mm/min | ||
Dehnung | 4 % Show Supplier Material materials with Dehnung of 4 % | dry | ISO 527-2/1A | 5mm/min | |
5 % Show Supplier Material materials with Dehnung of 5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 4.1 GPa Show Supplier Material materials with Elastizitätsmodul of 4.1 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
6.7 GPa Show Supplier Material materials with Elastizitätsmodul of 6.7 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 9.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9.5 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | 50%RH | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 45 kJ/m² | dry | ISO 179/1eU | |
23 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | dry | ISO 179/1eU | ||
23 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | 50%RH | ISO 179/1eU | ||
Zugfestigkeit | 90 MPa Show Supplier Material materials with Zugfestigkeit of 90 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
145 MPa Show Supplier Material materials with Zugfestigkeit of 145 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | 2 mm | IEC 60695-2-12 | ||||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | 2 mm | IEC 60695-2-13 | ||||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat-Erweichungstemperatur | 240 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 240 °C | ISO 306 | 50°C/h 50N | ||||
Wärmeformbeständigkeitstemperatur | 220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | ISO 75/2Af | 1.80 MPa | ||||
250 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 250 °C | ISO 75/2Bf | 0.45 MPa | |||||
Entflammbarkeit | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | 300/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.9 % Show Supplier Material materials with Schrumpfung of 0.9 % | 300/90/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Fillers | 20% Glass Fiber | |
Processing methods | Injection Molding |