Allgemein
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Dichte | 1.48 g/cm³ Show Supplier Material materials with Dichte of 1.48 g/cm³ | dry | ISO 1183 | ||
Wasserabsorption | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | ISO 62 | 2 mm | 24h immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 290 MPa Show Supplier Material materials with Biegefestigkeit of 290 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 11.8 GPa Show Supplier Material materials with Biegemodul of 11.8 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 1.6 % Show Supplier Material materials with Dehnung of 1.6 % | dry | ISO 527-2/1A | 5mm/min | |
Elastizitätsmodul | 13.5 GPa Show Supplier Material materials with Elastizitätsmodul of 13.5 GPa | dry | ISO 527-2/1A | 1mm/min | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 45 kJ/m² | dry | ISO 179/1eU | |
23 °C | 55 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 55 kJ/m² | dry | ISO 179/1eU | ||
Zugfestigkeit | 195 MPa Show Supplier Material materials with Zugfestigkeit of 195 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Schmelzpunkt | 312 °C Show Supplier Material materials with Schmelzpunkt of 312 °C | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 285 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 285 °C | ISO 75/2Af | 1.80 MPa | ||
Entflammbarkeit | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | 325/140/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.7 % Show Supplier Material materials with Schrumpfung of 0.7 % | 325/140/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 35% Glass Fiber | |
Processing methods | Injection Molding |