Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.14 g/cm³ Show Supplier Material materials with Dichte of 1.14 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 3 % Show Supplier Material materials with Moisture absorption of 3 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 10.2 % Show Supplier Material materials with Wasserabsorption of 10.2 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 65 MPa Show Supplier Material materials with Biegefestigkeit of 65 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 1.8 GPa Show Supplier Material materials with Biegemodul of 1.8 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
Elastizitätsmodul | 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 2.3 GPa | dry | ISO 527-2/1A | 1mm/min | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-2/1A | 50mm/min | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5.5 kJ/m² | dry | ISO 179/1eA | ||
Streckgrenze | 55 MPa Show Supplier Material materials with Streckgrenze of 55 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 650 °C Show Supplier Material materials with Glow Wire Flammability Index of 650 °C | 2 mm | IEC 60695-2-12 | ||||
Schmelzpunkt | 195 °C Show Supplier Material materials with Schmelzpunkt of 195 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat-Erweichungstemperatur | 70 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 70 °C | ISO 306 | 50°C/h 50N | ||||
Wärmeformbeständigkeitstemperatur | 50 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 50 °C | ISO 75/2Af | 1.80 MPa | ||||
Entflammbarkeit | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): <10 ,method: ISO 3795 and thickness tested (mm): 3 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Viscosity number | 195 cm³/gr Show Supplier Material materials with Viscosity number of 195 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Additives | Lubricants | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Processing methods | Injection Molding,Film Extrusion,Profile Extrusion |