Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.04 g/cm³ Show Supplier Material materials with Dichte of 1.04 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 0.9 % Show Supplier Material materials with Moisture absorption of 0.9 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 2.2 % Show Supplier Material materials with Wasserabsorption of 2.2 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 60 MPa Show Supplier Material materials with Biegefestigkeit of 60 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 1.6 GPa Show Supplier Material materials with Biegemodul of 1.6 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 100 % Show Supplier Material materials with Dehnung of 100 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
Elastizitätsmodul | 1.6 GPa Show Supplier Material materials with Elastizitätsmodul of 1.6 GPa | dry | ISO 527-2/1A | 1mm/min | |
Elongation at yield | 6 % Show Supplier Material materials with Elongation at yield of 6 % | dry | ISO 527-2/1A | 50mm/min | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | dry | ISO 179/1eA | |
23 °C | 45 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 45 kJ/m² | dry | ISO 179/1eA | ||
Streckgrenze | 46 MPa Show Supplier Material materials with Streckgrenze of 46 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Impact Modified | |
Processing methods | Injection Molding,Profile Extrusion |