Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.1 g/cm³ Show Supplier Material materials with Dichte of 1.1 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 2.5 % Show Supplier Material materials with Wasserabsorption of 2.5 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 25 MPa Show Supplier Material materials with Biegefestigkeit of 25 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 0.62 GPa Show Supplier Material materials with Biegemodul of 0.62 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 100 % Show Supplier Material materials with Dehnung of 100 % | dry | ISO 527-2/1A | min. | 50mm/min | nominal | |
300 % Show Supplier Material materials with Dehnung of 300 % | 50%RH | ISO 527-2/1A | min. | 50mm/min | nominal | ||
Elastizitätsmodul | 0.53 GPa Show Supplier Material materials with Elastizitätsmodul of 0.53 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
0.75 GPa Show Supplier Material materials with Elastizitätsmodul of 0.75 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation at yield | 55 % Show Supplier Material materials with Elongation at yield of 55 % | dry | ISO 527-2/1A | 50mm/min | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 25 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 25 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 35 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 35 kJ/m² | 50%RH | ISO 179/1eA | ||
Streckgrenze | 30 MPa Show Supplier Material materials with Streckgrenze of 30 MPa | 50%RH | ISO 527-2/1A | 50mm/min | |
40 MPa Show Supplier Material materials with Streckgrenze of 40 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 0.00013 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.00013 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse |
0.000136 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000136 1/K | ISO 11359-1/-2 | 23°C-55°C | |
Schmelzpunkt | 215 °C Show Supplier Material materials with Schmelzpunkt of 215 °C | ISO 11357-1/-3 | 10°C/min |
Wärmeformbeständigkeitstemperatur | 50 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 50 °C | ISO 75/2Af | 1.80 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Plasticizer | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Heat Stabilized | |
Processing methods | Injection Molding,Profile Extrusion |