Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.01 g/cm³ Show Supplier Material materials with Dichte of 1.01 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 0.8 % Show Supplier Material materials with Moisture absorption of 0.8 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 2 % Show Supplier Material materials with Wasserabsorption of 2 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 30 MPa Show Supplier Material materials with Biegefestigkeit of 30 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 0.75 GPa Show Supplier Material materials with Biegemodul of 0.75 GPa | dry | ISO 178 | 2mm/min | |
Elastizitätsmodul | 0.95 GPa Show Supplier Material materials with Elastizitätsmodul of 0.95 GPa | dry | ISO 527-2/1A | 1mm/min | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 68 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 68 kJ/m² | dry | ISO 179/1eA | |
23 °C | 75 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 75 kJ/m² | dry | ISO 179/1eA | ||
Streckgrenze | 31 MPa Show Supplier Material materials with Streckgrenze of 31 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 212 °C Show Supplier Material materials with Schmelzpunkt of 212 °C | 1e+12 mm | ISO 11357-1/-3 | 10°C/min |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Impact Modified, Heat Stabilized | |
Processing methods | Injection Molding,Profile Extrusion |