Allgemein
Property | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|
Dichte | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | dry | ISO 1183 | ||
Wasserabsorption | 0.7 % Show Supplier Material materials with Wasserabsorption of 0.7 % | ISO 62 | 2 mm | 24h immersion at 23°C | |
1.9 % Show Supplier Material materials with Wasserabsorption of 1.9 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 95 MPa Show Supplier Material materials with Biegefestigkeit of 95 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 3.1 GPa Show Supplier Material materials with Biegemodul of 3.1 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 20 % Show Supplier Material materials with Dehnung of 20 % | dry | ISO 527-2/1A | 50mm/min | nominal | |
Elastizitätsmodul | 3.2 GPa Show Supplier Material materials with Elastizitätsmodul of 3.2 GPa | dry | ISO 527-2/1A | 1mm/min | |
Elongation at yield | 11 % Show Supplier Material materials with Elongation at yield of 11 % | dry | ISO 527-2/1A | 50mm/min | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 4.2 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.2 kJ/m² | dry | ISO 179/1eA | |
Streckgrenze | 61 MPa Show Supplier Material materials with Streckgrenze of 61 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzpunkt | 213 °C Show Supplier Material materials with Schmelzpunkt of 213 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | 280/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | 280/60/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, Drinking Water, RoHS 2011/65/UE | |
Color | Black | |
Features | Hydrolysis Resistance | |
Fillers | 30% Glass Bead | |
Processing methods | Injection Molding |