Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.37 g/cm³ Show Supplier Material materials with Dichte of 1.37 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 2 % Show Supplier Material materials with Moisture absorption of 2 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 7.5 % Show Supplier Material materials with Wasserabsorption of 7.5 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 160 MPa Show Supplier Material materials with Biegefestigkeit of 160 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 7.2 GPa Show Supplier Material materials with Biegemodul of 7.2 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 2.7 % Show Supplier Material materials with Dehnung of 2.7 % | dry | ISO 527-2/1A | 5mm/min | |
10 % Show Supplier Material materials with Dehnung of 10 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 5 GPa Show Supplier Material materials with Elastizitätsmodul of 5 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
7.5 GPa Show Supplier Material materials with Elastizitätsmodul of 7.5 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 3.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5.5 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | 50%RH | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | dry | ISO 179/1eU | -30°C | |
43 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 43 kJ/m² | dry | ISO 179/1eU | 23°C | ||
50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Zugfestigkeit | 65 MPa Show Supplier Material materials with Zugfestigkeit of 65 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | 2 mm | IEC 60695-2-12 | ||||
Koeffizient der thermischen Ausdehnung | 3.1e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.1e-05 1/K | ISO 11359-1/-2 | 23°C-55°C | ||||
0.000104 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.000104 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |||||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat-Erweichungstemperatur | 205 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 205 °C | ISO 306 | 50°C/h 50N | ||||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | ISO 75/2Af | 1.80 MPa | ||||
215 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 215 °C | ISO 75/2Bf | 0.45 MPa | |||||
Entflammbarkeit | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Kriechstromfestigkeit | 500 V Show Supplier Material materials with Kriechstromfestigkeit of 500 V | dry | IEC 60112 | Sol.A |
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | 50%RH | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | 50%RH | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | 280/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 30% Glass Fiber and Mineral Powder | |
Processing methods | Injection Molding |