Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness |
---|---|---|---|---|---|
Dichte | 1.72 g/cm³ Show Supplier Material materials with Dichte of 1.72 g/cm³ | dry | ISO 1183 | ||
Moisture absorption | 23 °C | 1 % Show Supplier Material materials with Moisture absorption of 1 % | 50%RH | ISO 62 | 2 mm |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 320 MPa Show Supplier Material materials with Biegefestigkeit of 320 MPa | 50%RH | ISO 178 | 2mm/min | |
385 MPa Show Supplier Material materials with Biegefestigkeit of 385 MPa | dry | ISO 178 | 2mm/min | ||
Biegemodul | 17.9 GPa Show Supplier Material materials with Biegemodul of 17.9 GPa | 50%RH | ISO 178 | 2mm/min | |
18.8 GPa Show Supplier Material materials with Biegemodul of 18.8 GPa | dry | ISO 178 | 2mm/min | ||
Dehnung | 2.2 % Show Supplier Material materials with Dehnung of 2.2 % | dry | ISO 527-2/1A | 5mm/min | |
2.5 % Show Supplier Material materials with Dehnung of 2.5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 19.6 GPa Show Supplier Material materials with Elastizitätsmodul of 19.6 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
22.1 GPa Show Supplier Material materials with Elastizitätsmodul of 22.1 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 15.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 16 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | 50%RH | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m² | dry | ISO 179/1eU | 23°C | |
102 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 102 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Zugfestigkeit | 200 MPa Show Supplier Material materials with Zugfestigkeit of 200 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
245 MPa Show Supplier Material materials with Zugfestigkeit of 245 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % | 290/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | 290/80/60* | ISO 294-4 | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, RoHS 2011/65/UE | |
Color | Black | |
Features | Improved Fluiditiy, Hydrolysis Resistance, High Surface Aspect, Heat Stabilized | |
Fillers | 60% Glass Fiber | |
Processing methods | Injection Molding |