Allgemein
Property | Temperature | Value | Testing Standard | Condition | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.45 g/cm³ Show Supplier Material materials with Dichte of 1.45 g/cm³ | ISO 1183 | ||||
Moisture absorption | 23 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ISO 62 | 50%RH | 2 mm | |
Wasserabsorption | 0.3 % Show Supplier Material materials with Wasserabsorption of 0.3 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Biegefestigkeit | 175 MPa Show Supplier Material materials with Biegefestigkeit of 175 MPa | ISO 178 | 2mm/min | |
Biegemodul | 6 GPa Show Supplier Material materials with Biegemodul of 6 GPa | ISO 178 | 2mm/min | |
Dehnung | 3.4 % Show Supplier Material materials with Dehnung of 3.4 % | ISO 527-2/1A | 5mm/min | |
Elastizitätsmodul | 6.8 GPa Show Supplier Material materials with Elastizitätsmodul of 6.8 GPa | ISO 527-2/1A | 1mm/min | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 7.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7.5 kJ/m² | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | ISO 179/1eU | |
Zugfestigkeit | 120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | 2 mm | IEC 60695-2-12 | ||||
Koeffizient der thermischen Ausdehnung | 3e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3e-05 1/K | ISO 11359-1/-2 | 23°C-55°C | ||||
0.0001 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 0.0001 1/K | ISO 11359-1/-2 | 23°C-55°C, Transverse | |||||
Schmelzpunkt | 225 °C Show Supplier Material materials with Schmelzpunkt of 225 °C | ISO 11357-1/-3 | 10°C/min | ||||
Vicat-Erweichungstemperatur | 205 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 205 °C | ISO 306 | 50°C/h 50N | ||||
Wärmeformbeständigkeitstemperatur | 200 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 200 °C | ISO 75/2Af | 1.80 MPa | ||||
220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | ISO 75/2Bf | 0.45 MPa | |||||
Entflammbarkeit | Thickness tested (mm): 1.6, Class: HB, Standard: UL 94 |
Elektrisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Schmelzmassenflussrate | 20 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 20 g/10min | ISO 1133 | 250°C/2.16Kg | |
Schrumpfung | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | ISO 294-4 | 280/90/60* | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
1 % Show Supplier Material materials with Schrumpfung of 1 % | ISO 294-4 | 280/90/60* | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Fillers | 20% Glass Fiber | |
Processing methods | Injection Molding |