Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.4 g/cm³ Show Supplier Material materials with Dichte of 1.4 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 265 MPa Show Supplier Material materials with Biegefestigkeit of 265 MPa | dry | ISO 178 | 2mm/min | |
Biegemodul | 10.6 GPa Show Supplier Material materials with Biegemodul of 10.6 GPa | dry | ISO 178 | 2mm/min | |
Dehnung | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | dry | ISO 527-2/1A | 5mm/min | |
Elastizitätsmodul | 10.8 GPa Show Supplier Material materials with Elastizitätsmodul of 10.8 GPa | dry | ISO 527-2/1A | 1mm/min | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | 58 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 58 kJ/m² | dry | ISO 179/1eU | 23°C | |
Zugfestigkeit | 168 MPa Show Supplier Material materials with Zugfestigkeit of 168 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzpunkt | 261 °C Show Supplier Material materials with Schmelzpunkt of 261 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 28 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 28 cm³/10min | ISO 1133 | 275°C/5Kg |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 35% Glass Fiber | |
Processing methods | Injection Molding |