Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Dichte of 1.38 g/cm³ | ASTM D792 |
Wasseraufnahme, Gleichgewicht | 23.0 °C | 0.3 % Show Supplier Material materials with Wasseraufnahme, Gleichgewicht of 0.3 % | max., ASTM D4442 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 250 MPa Show Supplier Material materials with Biegefestigkeit of 250 MPa | ASTM D790 |
Biegemodul | 23.0 °C | 8.33 GPa Show Supplier Material materials with Biegemodul of 8.33 GPa | ASTM D790 |
Dehnung | 23.0 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | max., ASTM D638 |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 90 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 90 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 135 MPa Show Supplier Material materials with Zugfestigkeit of 135 MPa | ASTM D638 |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.2 - 0.4 % Show Supplier Material materials with Schrumpfung of 0.2 - 0.4 % | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Air filter housing, Automobiles curtain, Automobiles gear assembly, Automobiles-Rearview mirror Rotation Axes. Home appliances. Scooters-Scooters Exhaust Heat Shield. Electromechanical parts and accessories, Harware, Mechanical parts. Office Chair Base, Office Chair Caster, Office furniture. Sports equipment, Plug, Fan blades, Plastic screw, Gear, Bicycle brake disc, Nut. | |
Color | Black | |
Fillers | 33% Glass Fiber |