Heat deflection temperature, 1.80 MPa: 245 °C

Quick Comparison

Polyamide 66 (PA66)

Zytel® 70G25HSL NC010

Polyamide 66 (PA66)

Akulon® S223-G6

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF007SXP

Geliefert von:

Sabic

Polyamide 66 (PA66)

Zytel® 80G33HS1L BK104

Polyamide 66 (PA66)

Akulon® S223-HPG5

Geliefert von:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® NMX33

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 80G25HSLWSF BK275

Polyamide 66 (PA66)

EPLAMID 66 GFH 30 HS BK Q2D003 (PA66)

Geliefert von:

EPSAN

Polyamide 66 (PA66)

EPLAMID 66 GFS 15 HS NC Q1B501 (PA66)

Geliefert von:

EPSAN

Polyamide 66 (PA66)

EPLAMID 66 GFS 20 HS NC Q1C001 (PA66)

Geliefert von:

EPSAN

Polyamide 66 (PA66)

Akulon® SG-KGS6

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFN14

Geliefert von:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF007H

Geliefert von:

Sabic

Other Polyamide (PA)

Zytel® HTN53G60LRHF BK083

Polyamide 4T (PA4T)

ForTii® XS81B

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Akulon® S223-KG6

Geliefert von:

DSM Engineering Materials
Seite 1 von 2