Allgemein
Property | Value | Comment |
---|---|---|
Partikelgröße | 50 - 60 nm Show Supplier Material materials with Partikelgröße of 50 - 60 nm | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.47 % Show Supplier Material materials with Aluminium of 0.47 % | Average between 2 spots |
Kohlenstoff | 68.29 % Show Supplier Material materials with Kohlenstoff of 68.29 % | Average between 2 spots |
Silizium | 31.07 % Show Supplier Material materials with Silizium of 31.07 % | Average between 2 spots |
Technological properties
Property | ||
---|---|---|
Other | Summary of the EDX-analysis for SiC: The EDX-measurements clearly show that the powder mainly consist of SiC. Since the spot-to-spot analysis varies quite a lot it is indicated that the powder consists of unreacted carbon besides the pure Silicon carbide. |