Allgemein
Property | Value | Comment |
---|---|---|
Partikelgröße | 50 - 60 nm Show Supplier Material materials with Partikelgröße of 50 - 60 nm | max. |
Chemical properties
Technological properties
Property | ||
---|---|---|
Other | Summary of the EDX-analysis for SiC: The EDX-measurements show no signs of impurities besides oxygen. In comparison with other nano-graphite/graphene powders the oxygen content is remarkably low. |