Allgemein
Property | Value |
---|---|
Kohlenstoffbilanz | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq / T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Abmessung
Property | Value |
---|---|
Dimensions | Weight: 7 kg, 10 kg, 16 kg |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 0 - 8 % Show Supplier Material materials with Dehnung A50 of 0 - 8 % | according to DIN EN 1706 |
Härte, Brinell | 23.0 °C | 0 - 90 [-] Show Supplier Material materials with Härte, Brinell of 0 - 90 [-] | according to DIN EN 1706 |
Streckgrenze Rp 0,2 | 23.0 °C | 0 - 220 MPa Show Supplier Material materials with Streckgrenze Rp 0,2 of 0 - 220 MPa | according to DIN EN 1706 |
Zugfestigkeit | 23.0 °C | 0 - 320 MPa Show Supplier Material materials with Zugfestigkeit of 0 - 320 MPa | according to DIN EN 1706 |
Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Andere | 0 - 0.15 % Show Supplier Material materials with Andere of 0 - 0.15 % |
Eisen | 0 - 0.2 % Show Supplier Material materials with Eisen of 0 - 0.2 % |
Magnesium | 0.15 - 0.6 % Show Supplier Material materials with Magnesium of 0.15 - 0.6 % |
Mangan | 0.4 - 0.8 % Show Supplier Material materials with Mangan of 0.4 - 0.8 % |
Silizium | 9 - 11.5 % Show Supplier Material materials with Silizium of 9 - 11.5 % |
Titan | 0 - 0.15 % Show Supplier Material materials with Titan of 0 - 0.15 % |
Technological properties
Property | ||
---|---|---|
Application areas | Structural Applications | |
Processing history | Smelters: Sayanogorsk Aluminium Smelter (SAZ), Khakas Aluminium Smelter (KHAZ), Irkutsk Aluminium Smelter (IrKAZ) |