Allgemein
Property | Value |
---|---|
Kohlenstoffbilanz | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Abmessung
Property | Value |
---|---|
Länge | 400 - 7000 mm Show Supplier Material materials with Länge of 400 - 7000 mm |
Dimensions | Diameter = 152 mm (6”), 178 mm (7”), 203 mm (8”), 228 mm (9”), 254 mm (10”), 279 mm (11”), 306 mm (12”), 356 mm (14”), 406 mm (16”), 457 mm (18”). |
Mechanisch
Property | Temperature | Value |
---|---|---|
Zugfestigkeit | 23.0 °C | 200 - 265 MPa Show Supplier Material materials with Zugfestigkeit of 200 - 265 MPa |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 615 - 659 °C Show Supplier Material materials with Schmelzpunkt of 615 - 659 °C | Solidus (615-624°C); Liquidus (655-659°C) |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | Balance | ||
Andere | 0.15 % Show Supplier Material materials with Andere of 0.15 % | according to EN 573-3 | |
Chrom | 0.1 % Show Supplier Material materials with Chrom of 0.1 % | according to EN 573-3 | |
Eisen | 0.35 % Show Supplier Material materials with Eisen of 0.35 % | according to EN 573-3 | |
Kupfer | 0.1 % Show Supplier Material materials with Kupfer of 0.1 % | according to EN 573-3 | |
Magnesium | 0.45 - 0.9 % Show Supplier Material materials with Magnesium of 0.45 - 0.9 % | according to EN 573-3 | |
Mangan | 0.1 % Show Supplier Material materials with Mangan of 0.1 % | according to EN 573-3 | |
Silizium | 0.2 - 0.6 % Show Supplier Material materials with Silizium of 0.2 - 0.6 % | according to EN 573-3 | |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % | according to EN 573-3 | |
Zink | 0.1 % Show Supplier Material materials with Zink of 0.1 % | according to EN 573-3 |
Technological properties
Property | ||
---|---|---|
Application areas | Extrusion Applications | |
Processing history | Smelters: Sayanogorsk Aluminium Smelter (SAZ), Krasnoyarsk Aluminium Smelter (KRAZ), Kubikenborg Aluminium AB (KUBAL) |