Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.22 - 0.32 [-] Show Supplier Material materials with Coefficient of friction of 0.22 - 0.32 [-] | ||
Coefficient of friction, kinetic | 0.32 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.32 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.22 [-] Show Supplier Material materials with Coefficient of friction, static of 0.22 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.17 g/cm³ Show Supplier Material materials with Dichte of 1.17 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 68 MPa Show Supplier Material materials with Biegefestigkeit of 68 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 1.9 GPa Show Supplier Material materials with Biegemodul of 1.9 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 5.6 % Show Supplier Material materials with Dehnung of 5.6 % | ASTM D 638 | yield |
Impact strength, Izod notched, ASTM | 23.0 °C | 542 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 542 J/m | ASTM D 256 | -40°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1762 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1762 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 43 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 43 kJ/m² | ISO 180/1A | notched 80*10*4, -40°C |
Zugfestigkeit | 23.0 °C | 54 MPa Show Supplier Material materials with Zugfestigkeit of 54 MPa | ASTM D 638 | break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 120 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 120 °C | ASTM D 648 | 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.01E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.01E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 120 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 120 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.54E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.54E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283871- - <br> UL Recognized, 94HB Flame Class Rating: 1.2mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101283841- - |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Lab Ware and Clinical Diagnostics, Head Protection, Document Handling | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 100°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |