Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.22 - 0.31 [-] Show Supplier Material materials with Coefficient of friction of 0.22 - 0.31 [-] | ||
Coefficient of friction, kinetic | 0.31 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.31 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.22 [-] Show Supplier Material materials with Coefficient of friction, static of 0.22 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.17 g/cm³ Show Supplier Material materials with Dichte of 1.17 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.18 % Show Supplier Material materials with Moisture absorption of 0.18 % | ISO 62 | (23°C / 50% RH) |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 78 MPa Show Supplier Material materials with Biegefestigkeit of 78 MPa | ISO 178 | ||
Biegemodul | 23.0 °C | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ISO 178 | 2 mm/min | ||
Dehnung | 23.0 °C | 5.6 % Show Supplier Material materials with Dehnung of 5.6 % | ISO 527 | yield | ||
Elastizitätsmodul | 23.0 °C | 2.1 GPa Show Supplier Material materials with Elastizitätsmodul of 2.1 GPa | ISO 527 | 1 mm/min | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 704 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 704 J/m | ASTM D 256 | notched, 23°C | ||
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 58 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 58 kJ/m² | ISO 180/1A | 80*10*4, 23°C | ||
Zugfestigkeit | 23.0 °C | 51 MPa Show Supplier Material materials with Zugfestigkeit of 51 MPa | ISO 527 | yield | ||
Impact strength, Izod unnotched, ASTM | ASTM D 4812 | 23°C |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 140 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 140 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 128 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 128 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.5E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 128 - 140 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 128 - 140 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.6E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.6E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283866- - |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosures, Food Processor, Lab Ware and Clinical Diagnostics, Document Handling, Displays, Data Management, Aircraft Seating, Circuit Protection, ATM/Ticket Machine, Amusement Machine, Audio, Auto Aftermarket, Wireless Communications, Wiring Devices, Vacuum Cleaner, Personal Computing, Navigation Unit, Medical Device, Monitoring and Imaging, Refrigerator, Pharmaceutical Packaging & Drug Delivery, Photo/Video Camera, Surgical Devices, Respiratory, Semiconductor | |
Availability | Asia,Americas | |
Processing methods | Back Pressure: 0.2 to 0.3MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |