Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.4 g/cm³ Show Supplier Material materials with Dichte of 1.4 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 346 MPa Show Supplier Material materials with Biegefestigkeit of 346 MPa | ISO 178 |
Biegemodul | 23.0 °C | 17 GPa Show Supplier Material materials with Biegemodul of 17 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.7 % Show Supplier Material materials with Dehnung of 1.7 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 24.1 GPa Show Supplier Material materials with Elastizitätsmodul of 24.1 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 9 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 9 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 44 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 44 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 230 MPa Show Supplier Material materials with Zugfestigkeit of 230 MPa | ISO 527 | break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6.9E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.9E-6 1/K | ISO 11359-2 | 23°C to 60°C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 2.93E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 2.93E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: 0.77mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101284441- - |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.12 % Show Supplier Material materials with Schrumpfung of 0.12 % | ISO 294 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, Semiconductor, Power Boat, Circuit Protection | |
Availability | Europe,Americas | |
Processing methods | Mold Temperature: 175 to 190.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |