Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.74 g/cm³ Show Supplier Material materials with Dichte of 1.74 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.36 % Show Supplier Material materials with Wasserabsorption of 0.36 % | ISO 62-1 | (23°C/24hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 170 MPa Show Supplier Material materials with Biegefestigkeit of 170 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 11 GPa Show Supplier Material materials with Biegemodul of 11 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.7 % Show Supplier Material materials with Dehnung of 1.7 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 12 GPa Show Supplier Material materials with Elastizitätsmodul of 12 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 3 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 25 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 105 MPa Show Supplier Material materials with Zugfestigkeit of 105 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | nan | IEC 60695-10-2 | 165°C +/- 2°C | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | IEC 60695-2-13 | 1.6 mm | |||
Heat deflection temperature, 0.45 MPa | 208 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 208 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 185 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 185 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.72E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.72E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Relative temperature index, electrical | 120 °C Show Supplier Material materials with Relative temperature index, electrical of 120 °C | UL 746B | |||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | UL 746B | |||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |||
Thermal conductivity, through-plane | 23.0 °C | 1.1 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 1.1 W/(m·K) | ISO 22007-2 | ?80*3mm discs | ||
Vicat-Erweichungstemperatur | 205 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 205 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 185 - 208 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 185 - 208 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 1.3 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 1.3 W/(m·K) | ISO 22007-2 | ?80*3mm discs | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.04E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.04E-5 1/K | ISO 11359-2 | -30°C to 80°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101761336- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥1mm UL 94 <br> Glow Wire Ignitability Temperature, 1.0 mm: 800°C IEC 60695-2-13 <br> Glow Wire Ignitability Temperature, 1.5 mm: 775°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 15.9 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 15.9 kV/mm | ASTM D 149 | in oil, 1.6 mm |
High Amp Arc Ignition | 23.0 °C | 1 mm Show Supplier Material materials with High Amp Arc Ignition of 1 mm | ≥, UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 1 mm Show Supplier Material materials with Hot-Wire Ignition of 1 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 0 V Show Supplier Material materials with Kriechstromfestigkeit of 0 V | UL 746A | (UL) {PLC} |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | LED Lighting | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |