Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.76 g/cm³ Show Supplier Material materials with Dichte of 1.76 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 164 MPa Show Supplier Material materials with Biegefestigkeit of 164 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 11 GPa Show Supplier Material materials with Biegemodul of 11 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.5 % Show Supplier Material materials with Dehnung of 1.5 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 12.5 GPa Show Supplier Material materials with Elastizitätsmodul of 12.5 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 3 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 3 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 102 MPa Show Supplier Material materials with Zugfestigkeit of 102 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 185 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 185 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.72E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3.72E-5 1/K | ISO 11359-2 | 23°C to 80°C |
Thermal conductivity, through-plane | 23.0 °C | 0.99 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 0.99 W/(m·K) | ISO 22007-2 | ?80*3mm discs |
Wärmeformbeständigkeitstemperatur | 185 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 185 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 1.3 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 1.3 W/(m·K) | ISO 22007-2 | ?80*3mm discs |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7.34E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7.34E-5 1/K | ISO 11359-2 | 23°C to 80°C |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Wiring Devices, Wireless Communications, LED Lighting, Medical Device, Personal Computing | |
Availability | Asia | |
Processing methods | Back Pressure: 0.2 to 0.3MPa | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |