Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.9 g/cm³ Show Supplier Material materials with Dichte of 1.9 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 47 MPa Show Supplier Material materials with Biegefestigkeit of 47 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 11.2 GPa Show Supplier Material materials with Biegemodul of 11.2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 0.6 % Show Supplier Material materials with Dehnung of 0.6 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 12.2 GPa Show Supplier Material materials with Elastizitätsmodul of 12.2 GPa | ASTM D 638 | 5 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 25 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 25 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 44 MPa Show Supplier Material materials with Zugfestigkeit of 44 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 191 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 191 °C | ASTM D 648 | 6.4 mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.6E-5 1/K | ASTM E 831 | 40°C to 120°C |
Thermal conductivity, through-plane | 23.0 °C | 0.9 W/(m·K) Show Supplier Material materials with Thermal conductivity, through-plane of 0.9 W/(m·K) | ISO 22007-2 | ?80*3mm discs |
Wärmeformbeständigkeitstemperatur | 191 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 191 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 1.95 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 1.95 W/(m·K) | ISO 22007-2 | ?80*3mm discs |
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5.1E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5.1E-5 1/K | ASTM E 831 | 40°C to 120°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1.00E+15 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+15 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, LED Lighting, Medical Device, Non-LED Lighting, Wireless Communications | |
Availability | Europe,Asia | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |