Property | Temperature | Value | Comment |
---|---|---|---|
Wasserabsorption | 23.0 °C | 0.06 % Show Supplier Material materials with Wasserabsorption of 0.06 % | ASTM D 570 | (23°C/24hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 111 MPa Show Supplier Material materials with Biegefestigkeit of 111 MPa | ASTM D 790 | yld, 2.6 mm/min, 100 mm span |
Biegemodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | ASTM D 790 | 2.6 mm/min, 100 mm span |
Dehnung | 23.0 °C | 9.5 % Show Supplier Material materials with Dehnung of 9.5 % | ASTM D 638 | yld, Type I, 50 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 160 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 160 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 55 MPa Show Supplier Material materials with Zugfestigkeit of 55 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 133 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 133 °C | ASTM D 648 | 6.4 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 122 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 122 °C | ASTM D 648 | 6.4 mm, unannealed | |
Vicat-Erweichungstemperatur | 150 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 150 °C | ASTM D 1525 | Rate B/50 | |
Wärmeformbeständigkeitstemperatur | 122 - 133 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 122 - 133 °C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥2.5mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=237097- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 60Hz | 23.0 °C | 2.57 [-] Show Supplier Material materials with Dielectric constant, 60Hz of 2.57 [-] | ASTM D 150 | 50/60 Hz |
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 2.49 [-] Show Supplier Material materials with Dielektrizitätskonstante, 1 MHz of 2.49 [-] | ASTM D 150 |
Dissipation factor, 1MHz | 23.0 °C | 2.6E-3 [-] Show Supplier Material materials with Dissipation factor, 1MHz of 2.6E-3 [-] | ASTM D 150 | |
Dissipation factor, 50Hz | 23.0 °C | 5.2E-3 [-] Show Supplier Material materials with Dissipation factor, 50Hz of 5.2E-3 [-] | ASTM D 150 | 50/60 Hz |
Durchschlagfestigkeit | 23.0 °C | 18.8 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 18.8 kV/mm | ASTM D 149 | in oil, 3.2 mm |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Volume resistivity | 23.0 °C | 2.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 2.00E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Electronic Components, Enclosures, Electronics, Energy Management, Enclosure/Housing/Cover, Heavy Vehicles, Head Protection, Gas/Electric Oven, Industrial Material Handling, Freezer, Auto Aftermarket, Circuit Protection, Air Conditioning, Dishwasher, Displays, Document Handling, Data Management, Bottles, Coffee Maker/Espresso Machine, Washing Machine, Vacuum Cleaner, Swimming Pool/Spa, Wireless Communications, Personal Care, Non-LED Lighting, Personal Computing, Laundry Dryer, Meter Water, LED Lighting, Photovoltaic Components, Power Manangement, Pump, Refrigerator, Small Appliance, Rail | |
Availability | Europe,Asia,Americas | |
Processing methods | Mold Temperature: 70 to 100.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |