Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 68 MPa Show Supplier Material materials with Biegefestigkeit of 68 MPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2 GPa Show Supplier Material materials with Biegemodul of 2 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 4 % Show Supplier Material materials with Dehnung of 4 % | ISO 527 | yield, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 1.9 GPa Show Supplier Material materials with Elastizitätsmodul of 1.9 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 645 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 645 J/m | ASTM D 256 | notched, 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 60 J Show Supplier Material materials with Instrumented Impact, Total Energy of 60 J | ASTM D 3763 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 34 J Show Supplier Material materials with Instrumented Impact, at Peak of 34 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 645 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 645 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 42 MPa Show Supplier Material materials with Zugfestigkeit of 42 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 123 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 123 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 64 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 64 °C | ASTM D 648 | 3.2mm, unannealed | |
Vicat-Erweichungstemperatur | 136 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 136 °C | ASTM D 1525 | Rate B/120 | |
Wärmeformbeständigkeitstemperatur | 64 - 123 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 64 - 123 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104427473 - - <br> UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 11 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 11 g/10min | ASTM D 1238 | 250°C/5.0 kgf | |
Schmelzvolumenflussrate | 10 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 10 cm³/10min | ASTM D 1238 | MVR at 250°C/5 kg | |
Schrumpfung | 23.0 °C | 1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | SABIC method |
Schrumpfung, diagonal | 23.0 °C | 1.2 % Show Supplier Material materials with Schrumpfung, diagonal of 1.2 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Healthcare | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |