Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.25 - 0.29 [-] Show Supplier Material materials with Coefficient of friction of 0.25 - 0.29 [-] | ||
Coefficient of friction, kinetic | 0.29 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.29 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.25 [-] Show Supplier Material materials with Coefficient of friction, static of 0.25 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.36 g/cm³ Show Supplier Material materials with Dichte of 1.36 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.01 % Show Supplier Material materials with Moisture absorption of 0.01 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.36 [-] Show Supplier Material materials with Relative Dichte of 1.36 [-] | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 123 MPa Show Supplier Material materials with Biegefestigkeit of 123 MPa | ISO 178 | 2 mm/min |
Biegemodul | 23.0 °C | 2.9 GPa Show Supplier Material materials with Biegemodul of 2.9 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 15 % Show Supplier Material materials with Dehnung of 15 % | ISO 527 | break, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 3.1 GPa Show Supplier Material materials with Elastizitätsmodul of 3.1 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 76 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 76 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1230 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1230 J/m | ASTM D 4812 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | ISO 179/1eA | V-notch Edgew, 23°C, 80*10*4 sp=62mm |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 7 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 7 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 95 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 95 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 70 MPa Show Supplier Material materials with Zugfestigkeit of 70 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 172 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 172 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 148 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 148 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 4.9E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4.9E-5 1/K | ASTM E 831 | -40°C to 120°C |
Wärmeformbeständigkeitstemperatur | 148 - 172 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 148 - 172 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5.8E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5.8E-5 1/K | ASTM E 831 | -40°C to 120°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1GHz | 23.0 °C | 3 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 3 [-] | SABIC method | 1.1 GHz |
Dielektrizitätskonstante | 23.0 °C | 2.6E-3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 2.6E-3 [-] | SABIC method | 1.9 GHz |
Dissipation factor, 1GHz | 23.0 °C | 3.01 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 3.01 [-] | SABIC method | |
Verlustfaktor | 23.0 °C | 2.8E-3 [-] Show Supplier Material materials with Verlustfaktor of 2.8E-3 [-] | SABIC method |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors, Heavy Vehicles, Enclosures, Electronic Components, Oil/Gas | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120 to 150.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |