Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ISO 1183 |
Relative Dichte | 23.0 °C | 1.2 [-] Show Supplier Material materials with Relative Dichte of 1.2 [-] | ASTM D 792 |
Sauerstoffindex | 23.0 °C | 38 % Show Supplier Material materials with Sauerstoffindex of 38 % |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 84 MPa Show Supplier Material materials with Biegefestigkeit of 84 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.1 GPa Show Supplier Material materials with Biegemodul of 2.1 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 5.2 % Show Supplier Material materials with Dehnung of 5.2 % | ISO 527 | yield, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.2 GPa Show Supplier Material materials with Elastizitätsmodul of 2.2 GPa | ISO 527 | 1 mm/min |
Hardness, Rockwell L | 23.0 °C | 84 [-] Show Supplier Material materials with Hardness, Rockwell L of 84 [-] | ASTM D 785 |
Hardness, Rockwell R | 23.0 °C | 117 [-] Show Supplier Material materials with Hardness, Rockwell R of 117 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 700 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 700 J/m | ASTM D 256 | -40°C |
Instrumented Impact, Total Energy | 23.0 °C | 66 J Show Supplier Material materials with Instrumented Impact, Total Energy of 66 J | ASTM D 3763 | -30°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 69 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 73 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 73 kJ/m² | ISO 180/1A | 80*10*3, 23°C |
Zugfestigkeit | 23.0 °C | 54 MPa Show Supplier Material materials with Zugfestigkeit of 54 MPa | ISO 527 | yield, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 119 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 119 °C | ISO 75/Cf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 108 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 108 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.8E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.8E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 124 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 124 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 108 - 119 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 108 - 119 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 9.8E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 9.8E-5 1/K | ISO 11359-2 | 23°C to 80°C | ||
Entflammbarkeit | Glow Wire Ignitability Temperature, 1.0 mm: 850°C IEC 60695-2-13 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.6mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥3.0mm UL 94 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> Glow Wire Flammability Index 960°C, passes at: 1mm IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=104423704- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 10GHz | 23.0 °C | 2.84 [-] Show Supplier Material materials with Dielectric constant, 10GHz of 2.84 [-] | SABIC method |
Dielectric constant, 1GHz | 23.0 °C | 2.87 [-] Show Supplier Material materials with Dielectric constant, 1GHz of 2.87 [-] | SABIC method | 1.1 GHz |
Dielectric constant, 5GHz | 23.0 °C | 2.81 [-] Show Supplier Material materials with Dielectric constant, 5GHz of 2.81 [-] | SABIC method |
Dielektrizitätskonstante | 23.0 °C | 2.81 [-] Show Supplier Material materials with Dielektrizitätskonstante of 2.81 [-] | SABIC method | 1.9 GHz |
Dissipation factor, 1GHz | 23.0 °C | 6.4E-3 [-] Show Supplier Material materials with Dissipation factor, 1GHz of 6.4E-3 [-] | SABIC method | |
Dissipation factor, 5GHz | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Dissipation factor, 5GHz of 6E-3 [-] | SABIC method |
Sheet resistivity, ROA | 23.0 °C | 1.00E+16 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1.00E+16 Ω | >, ASTM D 257 |
Verlustfaktor | 23.0 °C | 6E-3 [-] Show Supplier Material materials with Verlustfaktor of 6E-3 [-] | SABIC method |
Volume resistivity | 23.0 °C | 1.00E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+16 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 12 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 12 g/10min | ASTM D 1238 | 300°C/1.2 kgf | |
Schmelzvolumenflussrate | 11 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 11 cm³/10min | ISO 1133 | MVR at 300°C/1.2 kg | |
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | SABIC method | 3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung, diagonal of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Building/Construction Sheet, Data Management, Data Transfer, Displays, Document Handling, Aerospace, Air Conditioning, Audio, Lawn/Garden, Heavy Vehicles, Freezer, Engine Cooling System, EV Infrastructure, Electronics, Energy Management, Enclosure/Housing/Cover, Enclosures, Electronic Components, Non-LED Lighting, Personal Computing, LED Lighting, Infrastructure, Small Appliance, Security/Detection, Respiratory, Photo/Video Camera, Vacuum Cleaner, Swimming Pool/Spa, Wiring Devices, Watch/Jewelry, Wearables, Wireless Communications, Wire & cable | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 110°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |