Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.43 - 0.45 [-] Show Supplier Material materials with Coefficient of friction of 0.43 - 0.45 [-] | ||
Coefficient of friction, kinetic | 0.45 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.45 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.43 [-] Show Supplier Material materials with Coefficient of friction, static of 0.43 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.62 g/cm³ Show Supplier Material materials with Dichte of 1.62 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.22 % Show Supplier Material materials with Moisture absorption of 0.22 % | ISO 62 | (23°C / 50% RH) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 248 MPa Show Supplier Material materials with Biegefestigkeit of 248 MPa | ISO 178 |
Biegemodul | 23.0 °C | 11.4 GPa Show Supplier Material materials with Biegemodul of 11.4 GPa | ISO 178 |
Dehnung | 23.0 °C | 2 % Show Supplier Material materials with Dehnung of 2 % | ISO 527 | break |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 13 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 46 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 46 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 168 MPa Show Supplier Material materials with Zugfestigkeit of 168 MPa | ISO 527 | break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 204 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 204 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.84E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.84E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 180 °C Show Supplier Material materials with Relative temperature index, electrical of 180 °C | UL 746B | |||
Relative temperature index, mechanical impact | 170 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 170 °C | UL 746B | |||
Relative temperature index, mechanical strength | 180 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 180 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 204 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 204 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 4E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 4E-5 1/K | ISO 11359-2 | 23°C to 60°C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101283889- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | ≥, UL 746A | PLC 4 |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | ≥, UL 746A | PLC 0 |
Kriechstromfestigkeit | 23.0 °C | 3 V Show Supplier Material materials with Kriechstromfestigkeit of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Enclosure/Housing/Cover, Electronic Components, EV Infrastructure, Circuit Protection, ATM/Ticket Machine, Data Transfer, Personal Computing | |
Availability | Europe,Asia,Americas | |
Processing methods | Front - Zone 3 Temperature: 365 to 375.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |