Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.27 g/cm³ Show Supplier Material materials with Dichte of 1.27 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 160 MPa Show Supplier Material materials with Biegefestigkeit of 160 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 3 GPa Show Supplier Material materials with Biegemodul of 3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 60 % Show Supplier Material materials with Dehnung of 60 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 3.3 GPa Show Supplier Material materials with Elastizitätsmodul of 3.3 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 34 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 34 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1335 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1335 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 34 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 34 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 106 MPa Show Supplier Material materials with Zugfestigkeit of 106 MPa | ASTM D 638 | yld, Type I, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 200 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 200 °C | ASTM D 648 | 6.4 mm, unannealed | |
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 200 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 200 °C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101339191- - <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.8mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.8mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Data Management | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |