Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.34 - 1.4 g/cm³ Show Supplier Material materials with Dichte of 1.34 - 1.4 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 133 MPa Show Supplier Material materials with Biegefestigkeit of 133 MPa | ISO 178 |
Biegemodul | 23.0 °C | 3.5 GPa Show Supplier Material materials with Biegemodul of 3.5 GPa | ISO 178 |
Dehnung | 23.0 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | ISO 527 | yield |
Elastizitätsmodul | 23.0 °C | 3.5 GPa Show Supplier Material materials with Elastizitätsmodul of 3.5 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 48 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 48 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1383 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1383 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 10 J Show Supplier Material materials with Instrumented Impact, at Peak of 10 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 73 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 73 kJ/m² | ISO 180/1U | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 106 MPa Show Supplier Material materials with Zugfestigkeit of 106 MPa | ISO 527 | yield |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 194 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 194 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm |
Wärmeformbeständigkeitstemperatur | 194 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 194 °C |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Monitoring and Imaging, Surgical Devices | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |