Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.33 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 248 MPa Show Supplier Material materials with Biegefestigkeit of 248 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 11.7 GPa Show Supplier Material materials with Biegemodul of 11.7 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 1.6 % Show Supplier Material materials with Dehnung of 1.6 % | ASTM D 638 | break |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 373 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 373 J/m | ASTM D 4812 | 23°C |
Zugfestigkeit | 23.0 °C | 165 MPa Show Supplier Material materials with Zugfestigkeit of 165 MPa | ASTM D 638 | break |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |
Relative temperature index, mechanical impact | 105 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | |
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282750- - <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101345232- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000000 Ω | ASTM D 257 |
Volume resistivity | 23.0 °C | 100 - 1000000 Ω·cm Show Supplier Material materials with Volume resistivity of 100 - 1000000 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Data Management, Battery Cell, Auto Aftermarket | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |