Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.57 g/cm³ Show Supplier Material materials with Dichte of 1.57 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 268 MPa Show Supplier Material materials with Biegefestigkeit of 268 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 15.9 GPa Show Supplier Material materials with Biegemodul of 15.9 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 1.5 % Show Supplier Material materials with Dehnung of 1.5 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 17.9 GPa Show Supplier Material materials with Elastizitätsmodul of 17.9 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 485 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 485 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 185 MPa Show Supplier Material materials with Zugfestigkeit of 185 MPa | ASTM D 638 | break |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 212 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 212 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.52E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.52E-5 1/K | ASTM E 831 | -40°C to 40°C |
Wärmeformbeständigkeitstemperatur | 212 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 212 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 2.34E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 2.34E-5 1/K | ASTM E 831 | -40°C to 40°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Volume resistivity | 23.0 °C | 1.00E+10 - 1.00E+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+10 - 1.00E+11 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Time: 4 to 6.0hrs | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |