Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.433 g/cm³ Show Supplier Material materials with Dichte of 1.433 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.11 % Show Supplier Material materials with Moisture absorption of 0.11 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Relative Dichte | 23.0 °C | 1.44 [-] Show Supplier Material materials with Relative Dichte of 1.44 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 364 MPa Show Supplier Material materials with Biegefestigkeit of 364 MPa | ISO 178 |
Biegemodul | 23.0 °C | 30.6 GPa Show Supplier Material materials with Biegemodul of 30.6 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 0.9 % Show Supplier Material materials with Dehnung of 0.9 % | ISO 527 | break, 5 mm/min |
Druckfestigkeit | 23.0 °C | 218 MPa Show Supplier Material materials with Druckfestigkeit of 218 MPa | SABIC method |
Elastizitätsmodul | 23.0 °C | 35.5 GPa Show Supplier Material materials with Elastizitätsmodul of 35.5 GPa | ISO 527 | 1 mm/min |
Härte, Rockwell M | 23.0 °C | 112 [-] Show Supplier Material materials with Härte, Rockwell M of 112 [-] | ASTM D 785 | |
Impact strength, Izod notched, ASTM | 23.0 °C | 64 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 64 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 560 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 560 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 7 J Show Supplier Material materials with Instrumented Impact, Total Energy of 7 J | ASTM D 3763 | 23°C |
Poissonzahl | 23.0 °C | 0.4 [-] Show Supplier Material materials with Poissonzahl of 0.4 [-] | ASTM E 132 |
Scherfestigkeit | 23.0 °C | 120 MPa Show Supplier Material materials with Scherfestigkeit of 120 MPa | ASTM D732 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 6 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 33 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 33 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Schubmodule | 23.0 °C | 4.7 GPa Show Supplier Material materials with Schubmodule of 4.7 GPa | ASTM D732 |
Zugfestigkeit | 23.0 °C | 247 MPa Show Supplier Material materials with Zugfestigkeit of 247 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 193 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 193 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3E-6 1/K | ASTM E 831 | -40°C to 150°C |
Wärmeformbeständigkeitstemperatur | 193 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 193 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 4E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 4E-5 1/K | ASTM E 831 | -40°C to 150°C |
Elektrisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 40 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 40 g/10min | ASTM D 1238 | 380°C/6.7 kgf | |
Schrumpfung | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % | ASTM D 955 | 24 hrs |
Schrumpfung, diagonal | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung, diagonal of 0.1 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |