Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 332 MPa Show Supplier Material materials with Biegefestigkeit of 332 MPa | ISO 178 |
Biegemodul | 23.0 °C | 23.9 GPa Show Supplier Material materials with Biegemodul of 23.9 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.1 % Show Supplier Material materials with Dehnung of 1.1 % | ISO 527 | break, 5 mm/min |
Druckfestigkeit | 23.0 °C | 231 MPa Show Supplier Material materials with Druckfestigkeit of 231 MPa | SABIC method |
Elastizitätsmodul | 23.0 °C | 29.3 GPa Show Supplier Material materials with Elastizitätsmodul of 29.3 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 82 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 82 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 713 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 713 J/m | ASTM D 4812 | 23°C |
Poissonzahl | 23.0 °C | 0.4 [-] Show Supplier Material materials with Poissonzahl of 0.4 [-] | ASTM E 132 |
Scherfestigkeit | 23.0 °C | 128 MPa Show Supplier Material materials with Scherfestigkeit of 128 MPa | ASTM D732 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 82 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 82 kJ/m² | ASTM D 256 | notched, 23°C |
Schubmodule | 23.0 °C | 4.7 GPa Show Supplier Material materials with Schubmodule of 4.7 GPa | ASTM D732 |
Zugfestigkeit | 23.0 °C | 252 MPa Show Supplier Material materials with Zugfestigkeit of 252 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 195 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 195 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5E-6 1/K | ASTM E 831 | -40°C to 150°C |
Wärmeformbeständigkeitstemperatur | 195 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 195 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 7E-6 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 7E-6 1/K | ASTM E 831 | -40°C to 150°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 1000 Ω | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 69 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 69 g/10min | ASTM D 1238 | 380°C/6.7 kgf | |
Schrumpfung | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung of 0.1 % | ASTM D 955 | 24 hrs |
Schrumpfung, diagonal | 23.0 °C | 0.1 % Show Supplier Material materials with Schrumpfung, diagonal of 0.1 % | ASTM D 955 | 24 hrs |
Technological properties
Property | ||
---|---|---|
Application areas | Air Cabin Interiors, Aircraft Seating | |
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |