Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.38 g/cm³ Show Supplier Material materials with Dichte of 1.38 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 269 MPa Show Supplier Material materials with Biegefestigkeit of 269 MPa | ISO 178 |
Biegemodul | 23.0 °C | 15.9 GPa Show Supplier Material materials with Biegemodul of 15.9 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.1 % Show Supplier Material materials with Dehnung of 1.1 % | ISO 527 | break |
Elastizitätsmodul | 23.0 °C | 20.2 GPa Show Supplier Material materials with Elastizitätsmodul of 20.2 GPa | ISO 527 | 1 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 6 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 6 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 26 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 26 kJ/m² | ISO 180/1U | unnotched 80*10*4 |
Zugfestigkeit | 23.0 °C | 219 MPa Show Supplier Material materials with Zugfestigkeit of 219 MPa | ISO 527 | break, 5 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 217 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 217 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |
Wärmeformbeständigkeitstemperatur | 217 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 217 °C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: 0.75mm UL 94 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282614- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 10000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 10000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Application areas | Aircraft Exteriors, Air Cabin Interiors | |
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |