Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 344 MPa Show Supplier Material materials with Biegefestigkeit of 344 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 15.8 GPa Show Supplier Material materials with Biegemodul of 15.8 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 19.1 GPa Show Supplier Material materials with Elastizitätsmodul of 19.1 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 109 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 109 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 711 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 711 J/m | ASTM D 4812 | 23°C |
Poissonzahl | 23.0 °C | 0.4 [-] Show Supplier Material materials with Poissonzahl of 0.4 [-] | ASTM E 132 |
Scherfestigkeit | 23.0 °C | 121.4 MPa Show Supplier Material materials with Scherfestigkeit of 121.4 MPa | ASTM D732 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 109 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 109 kJ/m² | ASTM D 256 | notched, 23°C |
Schubmodule | 23.0 °C | 4.4 GPa Show Supplier Material materials with Schubmodule of 4.4 GPa | ASTM D732 |
Zugfestigkeit | 23.0 °C | 245 MPa Show Supplier Material materials with Zugfestigkeit of 245 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 170 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 170 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.4E-6 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.4E-6 1/K | ISO 11359-2 | -40°C to 40°C |
Wärmeformbeständigkeitstemperatur | 170 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 170 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5.5E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5.5E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100000 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100000 - 1000000 Ω | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Aircraft Seating | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 150°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |