Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.43 g/cm³ Show Supplier Material materials with Dichte of 1.43 g/cm³ | ASTM D 792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 199 MPa Show Supplier Material materials with Biegefestigkeit of 199 MPa | ASTM D 790 |
Biegemodul | 23.0 °C | 8.4 GPa Show Supplier Material materials with Biegemodul of 8.4 GPa | ASTM D 790 |
Dehnung | 23.0 °C | 2.7 % Show Supplier Material materials with Dehnung of 2.7 % | ASTM D 638 | break |
Elastizitätsmodul | 23.0 °C | 8.3 GPa Show Supplier Material materials with Elastizitätsmodul of 8.3 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 192 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 192 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 967 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 967 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 192 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 192 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 126 MPa Show Supplier Material materials with Zugfestigkeit of 126 MPa | ASTM D 638 | break |
Thermisch
Technological properties
Property | ||
---|---|---|
Application areas | Heavy Vehicles, Food Transportation, Medical Device | |
Availability | Europe,Asia,Americas | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |