Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.31 g/cm³ Show Supplier Material materials with Dichte of 1.31 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Impact strength, Izod unnotched, ASTM | 23.0 °C | 550 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 550 J/m | ASTM D 4812 | 23°C | ||
Biegefestigkeit | ISO 178 | yield, 2 mm/min | ||||
Biegemodul | ISO 178 | 2 mm/min | ||||
Dehnung | ISO 527 | yield, 5 mm/min | ||||
Elastizitätsmodul | ISO 527 | 1 mm/min | ||||
Zugfestigkeit | ISO 527 | break, 5 mm/min |
Thermisch
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 0.45 MPa | 150 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 150 °C | ASTM D 648 | 3.2 mm, unannealed |
Heat deflection temperature, 1.80 MPa | 55 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 55 °C | ASTM D 648 | 3.2mm, unannealed |
Vicat-Erweichungstemperatur | 207 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 207 °C | ASTM D 1525 | Rate A/120 |
Wärmeformbeständigkeitstemperatur | 55 - 150 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 55 - 150 °C |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 20 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 20 cm³/10min | ISO 1133 | MVR at 250°C/2.16 kg | |
Schrumpfung | 23.0 °C | 1.8 % Show Supplier Material materials with Schrumpfung of 1.8 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive , Electronics | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 100 to 120.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |