Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.54 g/cm³ Show Supplier Material materials with Dichte of 1.54 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.54 [-] Show Supplier Material materials with Relative Dichte of 1.54 [-] | ASTM D 792 | |
Wasserabsorption | 23.0 °C | 0.09 % Show Supplier Material materials with Wasserabsorption of 0.09 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 210 MPa Show Supplier Material materials with Biegefestigkeit of 210 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 9.1 GPa Show Supplier Material materials with Biegemodul of 9.1 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 1.6 % Show Supplier Material materials with Dehnung of 1.6 % | ISO 527 | yield, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 10.7 GPa Show Supplier Material materials with Elastizitätsmodul of 10.7 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 83 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 83 J/m | ASTM D 256 | notched, -30°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 770 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 770 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 7 J Show Supplier Material materials with Instrumented Impact, Total Energy of 7 J | ASTM D 3763 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 14 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 14 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*4 sp=62mm, 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 8 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 8 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 139 MPa Show Supplier Material materials with Zugfestigkeit of 139 MPa | ISO 527 | yield, 5 mm/min |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Ball pressure temperature | 200 °C Show Supplier Material materials with Ball pressure temperature of 200 °C | IEC 60695-10-2 | approximate maximum | |
Heat deflection temperature, 0.45 MPa | 217 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 217 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |
Heat deflection temperature, 1.80 MPa | 203 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 203 °C | ASTM D 648 | 3.2mm, unannealed | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Wärmeformbeständigkeitstemperatur | 203 - 217 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 203 - 217 °C | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.9E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.9E-5 1/K | ISO 11359-2 | -40°C to 40°C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 23 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 23 kV/mm | ASTM D 149 | in air, 3.2 mm |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+15 Ω·cm | >, ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 52 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 52 g/10min | ASTM D 1238 | 250°C/5.0 kgf | |
Schmelzvolumenflussrate | 38 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 38 cm³/10min | ISO 1133 | MVR at 250°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Schrumpfung, diagonal | 23.0 °C | 0.8 % Show Supplier Material materials with Schrumpfung, diagonal of 0.8 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Personal Care, Small Appliance | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |