Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ISO 62 | (23°C / 50% RH) |
Relative Dichte | 23.0 °C | 1.19 [-] Show Supplier Material materials with Relative Dichte of 1.19 [-] | ASTM D 792 | |
Wasserabsorption | 23.0 °C | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | ISO 62-1 | (23°C/saturated) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 96 MPa Show Supplier Material materials with Biegefestigkeit of 96 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 90 % Show Supplier Material materials with Dehnung of 90 % | ISO 527 | break, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.5 GPa Show Supplier Material materials with Elastizitätsmodul of 2.5 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 100 J/m | ASTM D 256 | notched, -30°C |
Instrumented Impact, Total Energy | 23.0 °C | 65 J Show Supplier Material materials with Instrumented Impact, Total Energy of 65 J | ASTM D 3763 | 23°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | ISO 179/1eA | V-notch Edgew 80*10*3 sp=62mm, -30°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 20 kJ/m² | ISO 180/1A | 80*10*3, 23°C |
Zugfestigkeit | 23.0 °C | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Ball Pressure Test | PASS | IEC 60695-10-2 | 75°C +/- 2°C | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 0.45 MPa | 100 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 100 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 93 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 93 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.4E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.4E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 90 °C Show Supplier Material materials with Relative temperature index, electrical of 90 °C | UL 746B | |||
Relative temperature index, mechanical impact | 90 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 90 °C | UL 746B | |||
Relative temperature index, mechanical strength | 90 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 90 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 110 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 110 °C | ISO 306 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 93 - 100 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 93 - 100 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.2E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.2E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94V-1 Flame Class Rating: ≥0.6mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-2 Flame Class Rating: ≥0.4mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥0.75mm UL 94 <br> UL Recognized, 94-5VB Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> Glow Wire Ignitability Temperature, 1.5 mm: 800°C IEC 60695-2-13 <br> Glow Wire Flammability Index, 1.5 mm: 960°C IEC 60695-2-12 <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=642976- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with High Amp Arc Ignition of 0.75 mm | UL 746A | PLC 0 |
Hot-Wire Ignition | 23.0 °C | 0.75 mm Show Supplier Material materials with Hot-Wire Ignition of 0.75 mm | UL 746A | PLC 3 |
Kriechstromfestigkeit | 23.0 °C | 3 V Show Supplier Material materials with Kriechstromfestigkeit of 3 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 16 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 16 g/10min | ASTM D 1238 | 260°C/2.16 kgf | |
Schmelzvolumenflussrate | 15 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 15 cm³/10min | ISO 1133 | MVR at 260°C/2.16 kg | |
Schrumpfung | 23.0 °C | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device, LED Lighting, Medical Facility Infrastructure, Non-LED Lighting, Personal Computing, Power Manangement, Photovoltaic Components, Power Boat, Respiratory, Small Appliance, Wireless Communications, Wearables, Wiring Devices, Enclosures, Energy Management, Enclosure/Housing/Cover, Electronic Components, EV Infrastructure, Head Protection, Lab Ware and Clinical Diagnostics, Lawn/Garden, Displays, Data Management, Data Transfer, Battery System, Air Conditioning, Building Accessory, Circuit Protection, Audio | |
Availability | Europe,Asia,Americas | |
Processing methods | Nozzle Temperature: 265 to 300.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |