Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.29 g/cm³ Show Supplier Material materials with Dichte of 1.29 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 80 MPa Show Supplier Material materials with Biegefestigkeit of 80 MPa | ISO 178 |
Biegemodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | ISO 178 |
Dehnung | 23.0 °C | 4 - 8 % Show Supplier Material materials with Dehnung of 4 - 8 % | ISO 527 | break |
Elastizitätsmodul | 23.0 °C | 2.8 GPa Show Supplier Material materials with Elastizitätsmodul of 2.8 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 122 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 122 J/m | ASTM D 256 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1788 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1788 J/m | ASTM D 4812 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 11 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 11 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 85 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 85 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 57 MPa Show Supplier Material materials with Zugfestigkeit of 57 MPa | ISO 527 | yield |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 136 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 136 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 125 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 125 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.6E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5.6E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 80 °C Show Supplier Material materials with Relative temperature index, electrical of 80 °C | UL 746B | |||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | UL 746B | |||
Relative temperature index, mechanical strength | 115 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 115 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 125 - 136 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 125 - 136 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 6.7E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 6.7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101343783- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=101343784- - <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> UL Recognized, 94V-0 Flame Class Rating: ≥2mm UL 94 <br> UL Recognized, 94V-1 Flame Class Rating: ≥1.6mm UL 94 <br> UV-light, water exposure/immersion: F1- UL 746C |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100 - 1000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100 - 1000 Ω | ASTM D 257 |
Shielding effectiveness | 23.0 °C | 40 dB Show Supplier Material materials with Shielding effectiveness of 40 dB | SABIC method | @ 3mm |
Volume resistivity | 23.0 °C | 10000 Ω·cm Show Supplier Material materials with Volume resistivity of 10000 Ω·cm | ASTM D 257 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Personal Computing, Power Manangement, Enclosures, Electronic Components, Lab Ware and Clinical Diagnostics, Individual Equiptment, Data Transfer, Conveyor | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |