Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.28 - 0.34 [-] Show Supplier Material materials with Coefficient of friction of 0.28 - 0.34 [-] | ||
Coefficient of friction, kinetic | 0.34 [-] Show Supplier Material materials with Coefficient of friction, kinetic of 0.34 [-] | ASTM D 3702 Modified: Manual | |
Coefficient of friction, static | 0.28 [-] Show Supplier Material materials with Coefficient of friction, static of 0.28 [-] | ASTM D 3702 Modified: Manual | |
Dichte | 23.0 °C | 1.52 g/cm³ Show Supplier Material materials with Dichte of 1.52 g/cm³ | ISO 1183 |
Moisture absorption | 23.0 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ASTM D 570 | (23°C/50% RH/24 hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 239 MPa Show Supplier Material materials with Biegefestigkeit of 239 MPa | ISO 178 |
Biegemodul | 23.0 °C | 13 GPa Show Supplier Material materials with Biegemodul of 13 GPa | ISO 178 |
Dehnung | 23.0 °C | 1.6 % Show Supplier Material materials with Dehnung of 1.6 % | ISO 527 | break |
Elastizitätsmodul | 23.0 °C | 15.8 GPa Show Supplier Material materials with Elastizitätsmodul of 15.8 GPa | ISO 527 | 1 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 53 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 53 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 534 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 534 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, at Peak | 23.0 °C | 4 J Show Supplier Material materials with Instrumented Impact, at Peak of 4 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 5 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 5 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 32 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod ungekerbt of 32 kJ/m² | ISO 180/1U | unnotched 80*10*4, 23°C |
Zugfestigkeit | 23.0 °C | 162 MPa Show Supplier Material materials with Zugfestigkeit of 162 MPa | ISO 527 | break |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 218 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 218 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 198 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 198 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.9E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Wärmeformbeständigkeitstemperatur | 198 - 218 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 198 - 218 °C | ||||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 5.7E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 5.7E-5 1/K | ISO 11359-2 | -40°C to 40°C | ||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101343442- - <br> UL Recognized, 94V-0 Flame Class Rating: 1.5mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=103093570- - |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |