Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.15 [-] Show Supplier Material materials with Relative Dichte of 1.15 [-] | ASTM D 792 | |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 88 MPa Show Supplier Material materials with Biegefestigkeit of 88 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 100 % Show Supplier Material materials with Dehnung of 100 % | ASTM D 638 | brk, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 2.3 GPa | ASTM D 638 | 50 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 587 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 587 J/m | ASTM D 256 |
Instrumented Impact, Total Energy | 23.0 °C | 54 J Show Supplier Material materials with Instrumented Impact, Total Energy of 54 J | ASTM D 3763 | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 587 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 587 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 57 MPa Show Supplier Material materials with Zugfestigkeit of 57 MPa | ASTM D 638 | yld, Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | IEC 60695-2-12 | 3.5 mm | |||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | IEC 60695-2-13 | 3.5 mm | |||
Heat deflection temperature, 0.45 MPa | 129 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 129 °C | ASTM D 648 | 3.2 mm, unannealed | |||
Heat deflection temperature, 1.80 MPa | 112 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 112 °C | ASTM D 648 | 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.2E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.2E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 105 °C Show Supplier Material materials with Relative temperature index, electrical of 105 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 105 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 105 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 130 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 130 °C | ISO 306 | Rate B/50 | |||
Wärmeformbeständigkeitstemperatur | 112 - 129 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 112 - 129 °C | ||||
Entflammbarkeit | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=103956763- - <br> UL Recognized, 94HB Flame Class Rating: ≥0.75mm UL 94 <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=103938405- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.2 mm Show Supplier Material materials with High Amp Arc Ignition of 1.2 mm | ≥, UL 746A | PLC 1 |
Hot-Wire Ignition | 23.0 °C | 1.2 mm Show Supplier Material materials with Hot-Wire Ignition of 1.2 mm | ≥, UL 746A | PLC 3 |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 19 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 19 g/10min | ASTM D 1238 | 260°C/5.0 kgf | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 100 to 110.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |