Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 93 MPa Show Supplier Material materials with Biegefestigkeit of 93 MPa | ASTM D 790 | yld, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Biegemodul of 2.3 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 6.2 % Show Supplier Material materials with Dehnung of 6.2 % | ASTM D 638 | yld, Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.3 GPa Show Supplier Material materials with Elastizitätsmodul of 2.3 GPa | ASTM D 638 | 50 mm/min |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 854 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 854 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 68 MPa Show Supplier Material materials with Zugfestigkeit of 68 MPa | ASTM D 638 | brk, Type I, 50 mm/min |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 137 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 137 °C | ASTM D 648 | 3.2 mm, unannealed | |
Heat deflection temperature, 1.80 MPa | 126 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 126 °C | ASTM D 648 | 3.2mm, unannealed | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | UL 746B | |
Relative temperature index, mechanical impact | 130 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | |
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | |
Wärmeformbeständigkeitstemperatur | 126 - 137 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 126 - 137 °C | ||
Entflammbarkeit | UL Recognized, 94HB Flame Class Rating: ≥0.7mm UL 94 <br> UV-light, water exposure/immersion: F2- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=220937- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
High Amp Arc Ignition | 23.0 °C | 1.14 mm Show Supplier Material materials with High Amp Arc Ignition of 1.14 mm | ≥, UL 746A | PLC 2 |
High Volt Arc Track Rate | 23.0 °C | 2 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 2 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 1.5 mm Show Supplier Material materials with Hot-Wire Ignition of 1.5 mm | ≥, UL 746A | PLC 2 |
Kriechstromfestigkeit | 23.0 °C | 2 V Show Supplier Material materials with Kriechstromfestigkeit of 2 V | UL 746A | (UL) {PLC} |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | on tensile bar |
Technological properties
Property | ||
---|---|---|
Application areas | Wireless Communications, Wiring Devices, Sunglasses, Small Appliance, LED Lighting, Personal Computing, Non-LED Lighting, Personal Care, Enclosures, Enclosure/Housing/Cover, Electronics, Electronic Components, Game Player, Food Processor, Document Handling, Doors Hardware/Trim, Displays, Data Transfer, Data Management, Audio, Air Cabin Interiors | |
Availability | Europe,Americas | |
Processing methods | Drying Temperature: 120°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |